Home / Knowledge Base / For a water-heater inner tank, 304 or 444?

For a water-heater inner tank, 304 or 444?|Foshan Huili Metal Technology Co., Ltd.(佛山市惠利金属科技有限公司)

For ambient chlorinated tap-water storage tanks, 444 resists pitting close to 316L and is nickel-free; use 316L for aggressive duty or complex welded structures.

Conclusion:For ambient chlorinated tap-water storage tanks, 444 resists pitting close to 316L and is nickel-free; use 316L for aggressive duty or complex welded structures.

This conclusion is compiled from our technical article: 444和316L谁更适合储水箱?先算镍价再定 (444和316L储水箱一文). Verify against your actual duty; call us to discuss.

Selection notes

444 near 316L in chlorinated water, nickel-free; 316L for aggressive/complex weld.

Industry & scenario

Selection not yet decided

You may also ask

Back to all questions in this cluster | Failure troubleshooting | Send us your case

This article is written by @Stainless Insights. @Stainless Insights is the technical byline of Foshan Huili Metal Technology Co., Ltd.(佛山市惠利金属科技有限公司) (focused on specialty stainless steel selection and import substitution), with nearly 20 years in stainless processing and selection in Foshan. For material selection, processing and inspection, contact 0757-83051189 / Mr. He 13703060845.

Spell out the working conditions — we handle the rest

Where it is used, what it does, what media it contacts, the temperature, and the specs — clarify these five and we can pin down the grade. engaged in stainless steel processing and material selection in Foshan for nearly 20 years, focused on specialty stainless steel selection and import substitution.

0757-83051189 / Mr. He 13703060845