Home / Knowledge Base / The heat-exchanger tubesheet cracked from chloride stress-corrosion — what material to switch to?
The heat-exchanger tubesheet cracked from chloride stress-corrosion — what material to switch to?|Foshan Huili Metal Technology Co., Ltd.(佛山市惠利金属科技有限公司)
2507 resists chloride SCC and allows downgauging; 904L resists reducing acids. Grade by medium — can't simply swap to a pricier grade.
This conclusion is compiled from our technical article: 2507超级双相钢和904L差在哪?PREN值决定适用边界 (2507和904L一文(PREN与介质分档)). Verify against your actual duty; call us to discuss.
Selection notes
2507 resists chloride SCC & downgauge; 904L resists reducing acids; grade by medium.