For seawater/coastal service, prefer 2205 duplex; for milder duty needing good weldability use 316L — the key is chloride level and SCC.
This conclusion is compiled from our technical article: 海水环境该用2205还是316L?先看氯离子浓度再定档 (海水环境2205还是316L一文). Verify against your actual duty; call us to discuss.
Selection notes
High chloride → 2205 duplex (PREN≥34); mild+weldable → 316L; measure medium first.